轻轨                                                             

Nominal

Size

型号

Unit

Weight

单位重量

Rail Height

A

Base Width

B

Head Width

C

Head Height

D

Web Height

E

Base Height

F

Web Thickness

t

kg/m mm mm mm mm mm mm mm
JIS  6kg 5.98 50.80 50.80 25.40 14.29 27.78 8.73 4.76
JIS  9kg 8.94 63.50 63.50 32.10 17.48 35.72 10.30 5.90
JIS 10kg 10.10 66.67 66.67 34.13 18.26 37.30 11.11 6.35
JIS 12kg 12.20 69.85 69.85 38.10 19.85 37.70 12.30 7.54
JIS 15kg 15.20 79.37 79.37 42.86 22.22 43.65 13.50 8.33
JIS 22kg 22.30 93.66 93.66 50.80 26.99 50.00 16.67 10.72
JIS 30kg 30.10 107.95 107.95 60.33 30.95 57.55 19.45 12.30
JIS 37kg 37.20 122.24 122.24 62.71 36.12 64.69 21.43 13.49
  JIS 40kgN 40.90 140.00 122.00 64.00 41.00 73.50 25.30 14.00
  JIS 50kgN 50.40 153.00 127.00 65.00 49.00 74.00 30.00 15.00
JIS 60kg 60.80 174.00 145.00 65.00 49.00 94.90 30.10 16.50
UIC 60kg 60.34 172.00 150.00 74.30 51.00 89.50 31.50 16.50