钢板 (英寸)

Steel Plates ( in Inches)

Thickness

厚度

4' x 8'

( 1219 x 2438 )

4' x 16'

( 1219 x 4877 )

5' x 10'

( 1524 x 3048 )

5' x 20'

( 1524 x 6096 )

6' x 20'

( 1829 x 6096 )

8' x 20'

( 2438 x 6096 )

8' x 30'

( 2438 x 9144 )

inches kgs lbs kgs lbs kgs lbs kgs lbs kgs lbs kgs lbs kgs lbs

1/16

1/8

3/16

1/4

5/16

3/8

7/16

1/2

9/16

5/8

11/16

3/4

13/16

7/8

15/16

1

1 1/8

1 1/4

1 3/8

1 1/2

1 5/8

1 3/4

1 7/8

2

2 1/2

3

4

5

6

37.05

74.10

111.1

148.2

185.2

222.3

259.3

296.4

333.4

370.5

407.5

444.6

481.6

518.7

555.7

592.8

666.9

741.0

815.1

889.1

963.2

1037

1111

1186

1482

1778

2371

2964

3557

81.68

163.4

244.9

326.7

408.3

490.1

571.7

653.4

735.0

816.8

898.4

980.2

1062

1144

1225

1307

1470

1634

1797

1960

2123

2286

2449

2615

3267

3920

5227

6534

7842

74.10

148.2

222.3

296.4

370.5

444.6

518.7

592.8

666.9

741.0

815.0

889.1

963.2

1037

1111

1186

1334

1482

1630

1778

1926

2075

2223

2371

2964

3567

4742

5928

7113

163.4

326.7

490.1

653.4

816.8

980.2

1144

1307

1470

1634

1797

1960

2123

2286

2450

2615

2941

3267

3594

3920

4248

4572

4899

5229

6534

7840

10454

13069

15684

57.89

115.8

173.7

231.5

289.4

347.3

405.2

463.1

521.0

578.9

636.8

694.6

752.5

810.4

868.3

926.2

1042

1158

1274

1389

1505

1621

1737

1852

2315

2779

3705

4631

5557

127.6

255.3

382.9

510.6

638.0

765.7

893.3

1021

1149

1276

1404

1532

1659

1787

1914

2042

2297

2553

2809

3062

3318

3574

3829

4083

5106

6127

8168

10210

12251

-

-

347.3

463.1

578.9

694.6

810.4

926.2

1042

1158

1274

1389

1505

1621

1737

1852

2084

2315

2547

2779

3010

3242

3473

3705

4631

5557

7410

9262

11114

-

-

765.7

1021

1276

1532

1787

2042

2297

2553

2809

3062

3318

3574

3829

4083

4594

5106

5615

6127

6636

7147

7657

8168

10210

12251

16336

20419

24502

-

-

416.8

555.7

694.4

833.6

972.5

1111

1250

1389

1528

1667

1806

1945

2084

2223

2501

2779

3056

3334

3612

3890

4168

4446

5557

6669

8891

11114

13337

-

-

918.9

1225

1532

1838

2144

2449

2756

3062

3369

3675

3982

4288

4594

4901

5514

6127

6737

7350

7963

8576

9189

9802

12251

14703

19603

24502

29403

-

-

-

741.0

926.2

1111

1297

1482

1667

1852

2038

2223

2408

2593

2779

2964

3334

3705

4075

4446

4816

5187

5557

5928

7410

8892

11855

14819

17783

-

-

-

1634

2042

2449

2589

3267

3675

4083

4493

4901

5309

5717

6127

6534

7350

8168

8984

9802

10617

11435

12251

13069

16336

19603

26136

32670

39205

-

-

-

1111

1389

1667

1945

2223

2501

2779

3056

3334

3612

3890

4168

4446

5001

5557

6113

6669

7224

7780

8336

8892

11114

13337

17783

22229

26675

-

-

-

2450

3063

3675

4288

4901

5513

6126

6738

7351

7963

8576

9189

9801

11026

12251

13477

14702

15927

17152

18377

19602

24503

29403

39204

49006

58807

cheap nfl nike jerseys, wholesale nba jerseys, cheap nba jerseys, new 2013 cheap nba jerseys, michael kors outlet, michael kors handbags, michael kors bags, nike free run, cheap nike free run, nike free run australia, red bottom shoes, christian louboutin outlet, red bottoms, red bottoms for men, nike air max shoes, cheap air max shoes, cheap nike air max, air max 90, nike australia, nike free run 3, nike store, cheap nike shoes, nike free run 2, cheap nfl jerseys china , cheap nfl authentic jerseys, authentic nfl jerseys cheap, cheap authentic nfl jerseys, nba throwback jerseys, wholesale nba jerseys, new 2013 cheap nba jerseys, authentic nfl jerseys wholesale, cheap nfl nike jerseys, nike tn, tn requin, nike tn pas cher, nike air max pas cher, chanel outlet, chanel bags, chanel handbags nike blazer, nike blazer vintage, nike blazer femme, nike blazer pas cher, Nike Air Max tn, air max tn pas cher, nike air max 90, chaussure nike air max, nike tn pas cher, air jordan, air jordan pas cher, nike air jordan, air jordan femme, michael kors outlet, michael kors outlet online, michael kors purses, michael kors handbags, michael kors bags, red bottom shoes, christian louboutin outlet, red bottoms, red bottoms for men, Christian Louboutin Sale, michael kors Canada, michael kors outlet, michael kors purses, michael kors handbags, michael kors bags,