槽鋼

Serial Size

型号

Depth x Width

D x B

Thickness

厚度

Unit Weight

单位重量

Web

t

Flange

T

mm mm kg/m lb/ft

*50 x 50

5.0

6.0

3.86

2.59

75 x 40

76 x 38

5.0

5.1

7.0

6.8

6.92

6.70

4.65

4.50

100 x 50

102 x 51

5.0

6.1

7.5

7.6

9.36

10.4

6.29

7.00

125 x 65

127 x 64

6.0

6.4

8.0

9.2

13.4

14.9

9.00

10.0

150 x 75

150 x 75

152 x 76

152 x 89

6.5

9.0

6.4

7.1

10.0

12.5

9.0

11.6

18.6

24.0

17.9

23.8

12.5

16.1

12.0

16.0

180 x 75

180 x 90

178 x 76

178 x 89

7.0

7.5

6.6

7.6

10.5

12.5

10.3

12.3

21.4

27.1

20.8

26.8

14.4

18.2

14.0

18.0

200 x 75

200 x 80

200 x 90

203 x 76

203 x 89

8.5

7.5

8.0

7.1

8.1

11.5

11.0

13.5

11.2

12.9

25.3

24.6

30.3

23.8

29.8

17.0

16.5

20.4

16.0

20.0

230 x 80

230 x 90

229 x 76

229 x 89

8.0

8.5

7.6

8.6

12.0

13.5

11.2

13.3

28.4

33.1

26.1

32.8

19.1

22.2

17.5

22.0

250 x 80

250 x 90

250 x 90

254 x 76

254 x 89

8.0

9.0

11.0

8.1

9.1

12.5

13.0

14.5

10.9

13.6

30.2

34.6

40.2

28.3

35.7

20.3

23.3

27.0

19.0

24.0

280 x 100

280 x 100

9.0

11.5

13.0

16.0

38.8

48.2

26.1

32.4

300 x 90

300 x 90

300 x 90

305 x 89

305 x 102

9.0

10.0

12.0

10.2

10.2

13.0

15.5

16.0

13.7

14.8

38.1

43.8

48.6

41.7

46.2

25.6

29.4

32.1

28.0

31.0

380 x 100

380 x 100

380 x 100

381 x 102

10.5

13.0

13.0

10.4

16.0

16.5

20.0

16.3

54.5

62.0

67.3

55.1

36.6

41.7

45.2

37.0

432 x 102

12.2

16.8

65.5

44.0

       

Notes :

 ' * ' indicates Euronom 54 - 80

" Red " wordings indicates JIS G3192