扁钢

Width

宽度

Thickness

厚度

Unit Weight

单位重量

mm  mm kg/m

12

3.0

4.5

8.0

10.0

0.28

0.42

0.75

0.94

16

3.0

4.0

4.5

6.0

8.0

10.0

0.38

0.50

0.57

0.75

1.00

1.26

19

3.0

4.0

4.5

6.0

9.0

10.0

12.0

0.45

0.60

0.67

0.89

1.34

1.49

1.79

25

3.0

4.0

4.5

6.0

8.0

9.0

10.0

12.0

16.0

20.0

0.59

0.79

0.88

1.18

1.57

1.77

1.96

2.36

3.14

3.93

32

3.0

4.0

4.5

6.0

8.0

9.0

10.0

12.0

16.0

19.0

0.75

1.00

1.13

1.51

2.01

2.26

2.51

3.01

4.02

4.77

38

3.0

4.0

4.5

6.0

8.0

9.0

12.0

16.0

19.0

0.89

1.19

1.34

1.79

2.39

2.68

3.58

4.77

5.67

44

4.5

6.0

8.0

9.0

12.0

16.0

19.0

1.55

2.07

2.76

3.11

4.14

5.13

6.56

50

3.0

4.0

4.5

6.0

8.0

9.0

10.0

12.0

16.0

19.0

20.0

22.0

25.0

1.18

1.57

1.77

2.36

3.14

3.53

3.93

4.71

6.28

7.46

7.85

8.64

9.81

65

3.0

4.5

6.0

8.0

9.0

10.0

12.0

16.0

19.0

20.0

22.0

25.0

1.53

2.30

3.06

4.08

4.59

5.10

6.12

8.16

9.69

10.2

11.2

12.8

75

4.5

6.0

8.0

9.0

10.0

12.0

16.0

19.0

20.0

22.0

25.0

2.65

3.53

4.71

5.30

5.89

7.06

9.42

11.2

11.8

13.0

14.7

90

6.0

8.0

9.0

10.0

12.0

16.0

19.0

20.0

22.0

25.0

4.24

5.65

6.36

7.07

8.48

11.3

13.4

14.1

15.5

17.7

100

3.0

6.0

8.0

9.0

10.0

12.0

16.0

19.0

20.0

22.0

25.0

28.0

32.0

36.0

2.36

4.71

6.28

7.07

7.85

9.42

12.6

14.9

15.7

17.3

19.6

22.0

25.1

28.3

125

6.0

8.0

9.0

12.0

16.0

19.0

22.0

25.0

28.0

32.0

36.0

5.89

7.85

8.83

11.8

15.7

18.6

21.6

24.5

27.5

31.4

35.3

150

3.0

6.0

8.0

9.0

10.0

12.0

16.0

19.0

20.0

22.0

25.0

28.0

32.0

36.0

3.53

7.07

9.42

10.6

11.8

14.1

18.8

22.4

23.6

25.9

29.4

33.0

37.7

42.4

180

6.0

8.0

9.0

10.0

12.0

16.0

19.0

20.0

22.0

25.0

28.0

32.0

36.0

8.48

11.3

12.7

14.1

17.0

22.6

26.8

28.3

31.1

35.3

39.6

45.2

50.9

200

6.0

8.0

9.0

10.0

12.0

16.0

19.0

20.0

22.0

25.0

28.0

32.0

36.0

9.42

12.6

14.1

15.7

18.8

25.1

29.8

31.4

34.5

39.3

44.0

50.2

56.5

230

9.0

12.0

16.0

19.0

22.0

25.0

28.0

32.0

36.0

16.2

21.7

28.9

34.3

39.7

45.1

50.6

57.8

65.0

250

6.0

8.0

9.0

10.0

12.0

16.0

19.0

20.0

22.0

25.0

28.0

32.0

36.0

11.8

15.7

17.7

19.6

23.6

31.4

37.3

39.3

43.2

49.1

55.0

62.8

70.7

280

12.0

16.0

19.0

22.0

25.0

28.0

32.0

36.0

26.4

35.2

41.8

48.4

55.0

61.5

70.3

79.1

300

6.0

8.0

10.0

12.0

16.0

19.0

20.0

22.0

25.0

28.0

32.0

36.0

14.1

18.8

23.6

28.3

37.7

44.7

47.1

51.8

58.9

65.9

75.4

84.8