欧洲标准U型钢板椿

 Section

  型号

w

Mass 质量

(mm) (mm) (mm) (mm)

kg/m

            PU   6 600 113 7.5 6.4 45.6
            PU   8 600 140 8.0 8.0 54.5
            PU 12 600 180 9.8 9.0 66.1
            PU 16 600 190 12.0 9.0 74.7
            PU 20 600 215 12.4 10.0 84.3
            PU 25 600 226 14.2 10.0 93.6
            PU 32      600 226 19.5 11.0 114.1
            L 2S 500 170 12.3 9.0 69.7
            L 3S 500 200 14.1 10.0 78.9
            L 4S 500 200 15.5 10.0 86.2

 

规格                                                                    

                                                                                                                   (Properties minima unless stated)

Specification

规格

Yield Stress

屈服强度

N/mm2

Tensile Strength

抗拉强度

N/mm2

Elongation

伸长率

%

ASTM A328 270 485 17 on 8" Gauge Length
ASTM A570 Grade 50 345 450 18 on 8" Gauge Length
ASTM A690 345 485 18 on 8" Gauge Length
BS EN 10248 : 1996 S270GP 270 410 24 on Gauge Length = 5.65ÖSo
BS EN 10248 : 1996 S355GP 355 480 22 on Gauge Length = 5.65ÖSo