Nominal Size

型号

Unit weight

单位重量

Rail Height

A

Base Width

B

Head Width

C

Web Thickness

t

kg/m

mm

mm

mm

mm

U.I.C. 50

50.12

152.00

125.00

72.20

15.00

U.I.C. 54

54.75

159.00

140.00

72.20

16.00

U.I.C. 60

60.22

172.00

150.00

74.30

16.50

A.S.C.E. 40

20.09

88.90

88.90

47.63

9.92

A.S.C.E. 60

30.08

107.95

107.95

60.33

12.30

A.S.C.E. 75

37.18

122.24

122.24

62.71

13.49

A.S.C.E. 80

39.86

127.00

127.00

63.50

13.89