Nominal Size 型号 |
Unit weight 单位重量 |
Rail Height A |
Base Width B |
Head Width C |
Web Thickness t |
|
|
kg/m |
mm |
mm |
mm |
mm |
||
|
100 RE |
50.21 |
152.40 |
136.52 |
68.26 |
14.29 |
|
|
115 RE |
56.96 |
168.28 |
139.70 |
69.06 |
15.88 |
|
|
119 RE |
58.88 |
173.04 |
139.70 |
67.47 |
15.88 |
|
|
132 RE |
65.38 |
180.98 |
152.40 |
76.20 |
16.67 |
|
|
133 RE |
66.25 |
179.39 |
152.40 |
76.20 |
17.46 |
|
|
136 RE |
67.68 |
185.74 |
152.40 |
74.61 |
17.46 |
|
|
136 RE Modified Crowns |
CN |
67.71 |
186.53 |
152.40 |
74.61 |
17.46 |
|
BN |
67.42 |
187.74 |
152.40 |
74.61 |
17.46 |
|
|
Optimum Crown |
67.36 |
187.74 |
152.40 |
74.61 |
17.46 |
|
|
140 RE |
69.17 |
185.74 |
152.40 |
76.20 |
19.05 |
|