| 英国标准'O', 'R' & 'N'式 |
|
Nominal Size 型号 |
Unit weight 单位重量 |
Rail Height A |
Base Width B |
Head Width C |
Web Thickness t |
|
kg/m |
mm |
mm |
mm |
mm |
|
|
50 ' O' |
24.82 |
100.01 |
100.01 |
52.39 |
10.32 |
|
80 'O' |
39.74 |
127.00 |
127.00 |
63.50 |
13.89 |
|
60 R |
29.85 |
114.30 |
109.54 |
57.15 |
11.11 |
|
75 R |
37.09 |
128.59 |
122.24 |
61.91 |
13.10 |
|
80 R |
39.72 |
133.35 |
127.00 |
63.50 |
13.49 |
|
90 R |
44.58 |
142.88 |
136.53 |
66.67 |
13.89 |
|
95 R |
47.21 |
147.64 |
141.29 |
68.26 |
14.29 |
|
100 R |
49.60 |
152.40 |
146.05 |
69.85 |
14.29 |
|
95 N |
47.27 |
147.64 |
139.70 |
69.85 |
13.89 |