镀锌钢板/卷(日本标准)
![]()
![]()
热轧钢板/卷
![]()
(Properties minima unless stated)
|
Symbol of Grade 钢号 |
Nominal Thickness 厚度 |
Quality 品质 |
Bendability 可弯曲度(Bending Angle 180º) |
Yield Stress 屈服强度 N/mm2 |
Tensile Strength 抗拉强度 N/mm2 |
Elongation 伸长率 % (minimum) 最小 |
Test Piece 测试片 |
||||||||
|
t<1.6 |
1.6£t<3.0 |
3.0£t |
|||||||||||||
|
Z27 or less |
Z35 |
Z45, Z60 |
Z27 or less |
Z35 |
Z45, Z60 |
Z27 or less |
Z35 |
Z45, Z60 |
|||||||
|
SGHC |
1.60£t£6.0 |
Commercial |
1 |
1 |
2 |
1 |
2 |
2 |
2 |
2 |
2 |
- |
- |
- |
No.5 in rolling direction |
|
SGH340 |
1.60£t£6.0 |
Structural |
1 |
1 |
2 |
1 |
1 |
2 |
2 |
2 |
3 |
245 |
340 |
20 |
|
|
SGH400 |
1.60£t£6.0 |
Structural |
2 |
2 |
2 |
2 |
2 |
2 |
3 |
3 |
3 |
295 |
400 |
18 |
|
|
SGH440 |
1.60£t£6.0 |
Structural |
3 |
3 |
3 |
3 |
3 |
3 |
3 |
3 |
3 |
335 |
440 |
||
|
SGH490 |
1.60£t£6.0 |
Structural |
3 |
3 |
3 |
3 |
3 |
3 |
3 |
3 |
3 |
365 |
490 |
16 |
|
|
SGH540 |
1.60£t£6.0 |
Structural |
3 |
3 |
3 |
3 |
3 |
3 |
3 |
3 |
3 |
400 |
540 |
||
冷轧钢板/卷
![]()
(Properties minima unless stated)
|
Symbol of Grade 钢号 |
Nominal Thickness 厚度 |
Quality 品质 |
Bendability 可弯曲度 (Bending Angle 180º) |
Yield Stress 屈服强度 N/mm2 |
Tensile Strength 抗拉强度 N/mm2 |
Elongation 伸长率 % (minimum 最小) |
Test Piece 测试片 |
|||||||||||||
|
t<1.6 |
1.6£t<3.0 |
3.0£t |
Nominal Thickness 公称厚度 (mm) | |||||||||||||||||
|
Z27 or less |
Z35 |
Z45, Z60 |
Z27 or less |
Z35 |
Z45, Z60 |
Z27 or less |
Z35 |
Z45, Z60 |
³0.25 <0.40 |
³0.40 <0.60 |
³0.60 <1.0 |
³1.0 <1.6 |
³1.6 <2.5 |
³2.5 |
||||||
| SGCC | 0.25£t£3.2 |
Commercial |
1 | 1 | 2 | 1 | 2 | 2 | 2 | 2 | 2 | - | - | - | - | - | - | - | - |
No.5 in rolling direction |
| SGCH | 0.11£t£1.0 |
Commercial hard class |
- | - | - | - | - | - | - | - | - | - | - | - | - | - | - | - | - | |
| SGCD1 | 0.40£t£2.3 |
Drawing, class 1 |
1 | - | - | 1 | - | - | - | - | - | - | 270 | - | 34 | 36 | 37 | 38 | - | |
| SGCD2 | 0.40£t£2.3 |
Drawing, class 2 |
0 | - | - | 0 | - | - | - | - | - | - | 270 | - | 36 | 38 | 39 | 40 | - | |
| SGCD3 | 0.60£t£2.3 |
Drawing, class 3 |
0 | - | - | 0 | - | - | - | - | - | - | 270 | - | 38 | 40 | 41 | 42 | - | |
| SGC340 | 0.25£t£3.2 |
Structural |
1 | 1 | 2 | 1 | 1 | 2 | 2 | 2 | 3 | 245 | 340 | 20 | 20 | 20 | 20 | 20 | 20 | |
| SGC400 | 0.25£t£3.2 |
Structural |
2 | 2 | 2 | 2 | 2 | 2 | 3 | 3 | 3 | 295 | 400 | 18 | 18 | 18 | 18 | 18 | 18 | |
| SGC440 | 0.25£t£3.2 |
Structural |
3 | 3 | 3 | 3 | 3 | 3 | 3 | 3 | 3 | 335 | 440 | 18 | 18 | 18 | 18 | 18 | 18 | |
| SGC490 | 365 | 490 | 16 | 16 | 16 | 16 | 16 | 16 | ||||||||||||
| SGC570 | 0.25£t£2.0 |
Structural |
- | - | - | - | - | - | - | - | - | 560 | 570 | - | - | - | - | - | - | |
Remark : For nominal thicknesses less than 0.25mm, tension test shall, as a rule, not be conducted