Type of Steel |
Strength ( Minimum Yield Point) N / mm2 |
Lloyd's Register of Shipping LR |
Bureau Veritas BV |
Germanischer Lioyd GL |
American Bureau of shipping AB |
Detnorske Veritas NV |
USSR Register of shipping SR |
|
MS |
235 |
A, B, D, E |
A B, D, E |
A, B, D, E |
A, B, D, E |
A, B, D, E |
A, B, D, E |
|
HTS |
265 |
|
|
|
|
A 27S D 27S E 27S |
|
|
315 |
AH 32 DH 32 EH 32 FH 32 |
AH 32 DH 32 EH 32 |
A 32 D 32 E 32 |
AH 32 DH 32 EH 32 FH 32 |
A 32 D 32 E 32 F 32 |
A 32 D 32 E 32 |
|
|
345 |
AH 34S DH 34S EH 34S |
|
|
|
|
|
|
|
355 |
AH 36 DH 36 EH 36 FH 36 |
AH 36 DH 36 EH 36 |
A 36 D 36 E 36 |
Ah 36 DH 36 EH 36 FH 36 |
A 36 D 36 E 36 F 36 |
A 36 D 36 E 36 |
|
|
390 |
AH 40 DH 40 EH 40 FH 40 |
|
|
AH 40 DH 40 EH 40 FH 40 |
A 40 D 40 E 40 F 40 |
|