| mm | kg/m2 | kgs | lbs | kgs | lbs | kgs | lbs |
| 2.3 | 19.73 | 58.64 | 129.3 | 91.65 | 202.1 | 183.3 | 404.1 |
| 3.0 | 25.15 | 74.74 | 164.8 | 116.8 | 257.5 | 233.7 | 515.2 |
| 3.2 | 26.79 | 79.62 | 175.5 | 124.4 | 274.3 | 248.9 | 548.7 |
| 4.5 | 36.99 | 109.9 | 242.3 | 171.8 | 378.8 | 343.6 | 757.5 |
| 6.0 | 48.77 | 144.9 | 319.4 | 226.5 | 499.3 | 453.1 | 998.9 |
| 7.5 | 60.53 | 179.9 | 396.6 | 281.2 | 619.9 | 562.3 | 1240 |
| 8.0 | 64.47 | 191.6 | 422.4 | 299.5 | 660.3 | 598.9 | 1320 |
| 9.0 | 72.32 | 214.9 | 473.8 | 335.9 | 740.5 | 671.9 | 1481 |
| 10.0 | 80.17 | 238.3 | 525.4 | 372.4 | 821.0 | 744.8 | 1642 |
| 12.0 | 95.87 | 284.9 | 628.1 | 445.3 | 981.7 | 890.7 | 1964 |
|
巴西标准 |
|
|
|
Thickness 厚度 |
Unit Weight 单位重量 |
4' x
8'
( 1219 x 2438 ) |
5' x
10'
( 1524 x 3048 ) |
5' x
20'
( 1524 x 6096 ) |
|||
| mm | kg/m2 | kgs | lbs | kgs | lbs | kgs | lbs |
| 4.5 | 36.63 | 108.9 | 240.0 | 170.2 | 375.1 | 340.3 | 750.2 |
| 5.0 | 40.56 | 120.5 | 265.7 | 188.4 | 415.3 | 376.8 | 830.6 |
| 6.0 | 48.41 | 143.9 | 317.1 | 224.8 | 495.7 | 449.7 | 991.4 |
| 7.5 | 60.18 | 178.9 | 394.3 | 279.5 | 616.3 | 559.1 | 1233 |
| 8.0 | 64.11 | 190.5 | 420.0 | 297.8 | 656.5 | 595.6 | 1313 |
| 9.0 | 71.96 | 213.8 | 471.4 | 334.2 | 736.9 | 668.5 | 1474 |
| 10.0 | 79.81 | 237.2 | 522.9 | 370.7 | 817.3 | 741.4 | 1635 |
| 12.0 | 95.51 | 283.8 | 625.7 | 443.6 | 978.0 | 887.3 | 1956 |