英国标准钢管

钢管

镀锌钢管

Nominal Size

型号

Outside Diameter

外径

Wall Thickness

壁厚

max

最大

min

最小

in (mm) in mm in mm in mm
l1/8"     (6mm)  0.398 10.1 0.382 9.7 0.072 1.83
l1/4"     (8mm)  0.535 13.6 0.520 13.2 0.072 1.83
l3/8"   (10mm)  0.673 17.1 0.657 16.7 0.072 1.83
1/2"   (15mm)  0.841 21.4 0.825 21.0 0.079 2.0
3/4"   (20mm)  1.059 26.9 1.041 26.4 0.091 2.3
1"   (25mm)  1.328 33.8 1.309 33.2 0.102 2.6
1 1/4"   (32mm)  1.670 42.5 1.650 41.9 0.102 2.6
1 1/2"   (40mm)  1.903 48.4 1.882 47.8 0.114 2.9
2"   (50mm)  2.370 60.2 2.347 59.6 0.114 2.9
2 1/2"   (65mm)  2.991 76.0 2.960 75.2 0.126 3.2
3"   (80mm)  3.491 88.7 3.460 87.9 0.126 3.2

4" (100mm) 

4.481

113.9

4.450

113.0

0.142

3.6

 

Nominal Size

型号

Outside Diameter

外径

Wall Thickness

壁厚

max

最大

min

最小

in (mm) in mm in mm in mm
l1/8"     (6mm)  0.409 10.4 0.386 9.8 0.080 2.03
l1/4"     (8mm)  0.547 13.9 0.524 13.3 0.093 2.35
l3/8"   (10mm)  0.685 17.4 0.661 16.8 0.093 2.35
1/2"   (15mm)  0.856 21.7 0.831 21.1 0.102 2.6
3/4"   (20mm)  1.072 27.2 1.047 26.6 0.102 2.6
1"   (25mm)  1.346 34.2 1.316 33.4 0.126 3.2
1 1/4"   (32mm)  1.687 42.9 1.657 42.1 0.126 3.2
1 1/2"   (40mm)  1.919 48.8 1.889 48.0 0.126 3.2
2"   (50mm)  2.394 60.8 2.354 59.8 0.142 3.6
2 1/2"   (65mm)  3.014 76.6 2.969 75.4 0.142 3.6
3"   (80mm)  3.524 89.5 3.469 88.1 0.157 4.0

4" (100mm) 

4.524 114.9 4.459 113.3 0.177 4.5
5" (125mm)  5.334 140.6 5.459 138.7 0.197 5.0
6" (150mm)  6.539 166.1 6.459 164.1 0.197 5.0

 

Nominal Size

型号

Outside Diameter

外径

Wall Thickness

壁厚

max

最大

min

最小

in (mm) in mm in mm in mm
l1/8"     (6mm)  0.409 10.4 0.386 9.8 0.104 2.65
l1/4"     (8mm)  0.547 13.9 0.524 13.3 0.116 2.94
l3/8"   (10mm)  0.685 17.4 0.661 16.8 0.116 2.94
1/2"   (15mm)  0.856 21.7 0.831 21.1 0.126 3.2
3/4"   (20mm)  1.072 27.2 1.047 26.6 0.126 3.2
1"   (25mm)  1.346 34.2 1.316 33.4 0.157 4.0
11/4"   (32mm)  1.687 42.9 1.657 42.1 0.157 4.0
11/2"   (40mm)  1.919 48.8 1.889 48.0 0.157 4.0
2"   (50mm)  2.394 60.8 2.354 59.8 0.177 4.5
2 1/2"   (65mm)  3.014 76.6 2.969 75.4 0.177 4.5
3"   (80mm)  3.524 89.5 3.469 88.1 0.197 5.0

4" (100mm) 

4.524 114.9 4.459 113.3 0.213 5.4
5" (125mm)  5.534 140.6 5.459 138.7 0.213 5.4
6" (150mm)  6.539 166.1 6.459 164.1 0.213 5.4