日本标准不锈钢管 |
|
|
|
Nominal Diameter 公称口径 |
Outside Diameter 外径 |
Nominal Wall Thickness 公称壁厚 |
|||
|
Wall Thickness 壁厚 |
Weight (kg/m) 重量 |
||||
|
A |
B |
Grade 钢号 |
|||
|
304 304H 304L 321 321H
|
309 309S 310 310S 316 316H 316L 316Ti 317 317L 347 347H |
||||
|
mm |
in |
mm |
mm |
||
|
6 |
1/8 |
10.5 |
1.0 |
0.237 |
0.238 |
| 8 | 1/4 | 13.8 | 1.2 | 0.377 | 0.379 |
| 10 | 3/8 | 17.3 | 1.2 | 0.481 | 0.484 |
| 15 | 1/2 | 21.7 | 1.65 | 0.824 | 0.829 |
| 20 | 3/4 | 27.2 | 1.65 | 1.05 | 1.06 |
| 25 | 1 | 34.0 | 1.65 | 1.33 | 1.34 |
| 32 | 1 1/4 | 42.7 | 1.65 | 1.69 | 1.70 |
| 40 | 1 1/2 | 48.6 | 1.65 | 1.93 | 1.94 |
| 50 | 2 | 60.5 | 1.65 | 2.42 | 2.43 |
| 65 | 2 1/2 | 76.3 | 2.1 | 3.88 | 3.91 |
| 80 | 3 | 89.1 | 2.1 | 4.55 | 4.58 |
| 90 | 3 1/2 | 101.6 | 2.1 | 5.20 | 5.24 |
| 100 | 4 | 114.3 | 2.1 | 5.87 | 5.91 |
| 125 | 5 | 139.8 | 2.8 | 9.56 | 9.62 |
| 150 | 6 | 165.2 | 2.8 | 11.3 | 11.4 |
| 200 | 8 | 216.3 | 2.8 | 14.9 | 15.0 |
| 250 | 10 | 267.4 | 3.4 | 22.4 | 22.5 |
| 300 | 12 | 318.5 | 4.0 | 31.3 | 31.5 |
|
|
|
Nominal Diameter 公称口径 |
Outside Diameter 外径 |
Nominal Wall Thickness 公称壁厚 |
|||
|
Wall Thickness 壁厚 |
Weight (kg/m) 重量 |
||||
|
A |
B |
Grade 钢号 |
|||
|
304 304H 304L 321 321H
|
309 309S 310 310S 316 316H 316L 316Ti 317 317L 347 347H |
||||
|
mm |
in |
mm |
mm |
||
|
6 |
1/8 |
10.5 |
1.2 |
0.278 |
0.280 |
| 8 | 1/4 | 13.8 | 1.65 | 0.499 | 0.503 |
| 10 | 3/8 | 17.3 | 1.65 | 0.643 | 0.647 |
| 15 | 1/2 | 21.7 | 2.1 | 1.03 | 1.03 |
| 20 | 3/4 | 27.2 | 2.1 | 1.31 | 1.32 |
| 25 | 1 | 34.0 | 2.8 | 2.18 | 2.19 |
| 32 | 1 1/4 | 42.7 | 2.8 | 2.78 | 2.80 |
| 40 | 1 1/2 | 48.6 | 2.8 | 3.19 | 3.21 |
| 50 | 2 | 60.5 | 2.8 | 4.02 | 4.05 |
| 65 | 2 1/2 | 76.3 | 3.0 | 5.48 | 5.51 |
| 80 | 3 | 89.1 | 3.0 | 6.43 | 6.48 |
| 90 | 3 1/2 | 101.6 | 3.0 | 7.37 | 7.42 |
| 100 | 4 | 114.3 | 3.0 | 8.32 | 8.37 |
| 125 | 5 | 139.8 | 3.4 | 11.6 | 11.6 |
| 150 | 6 | 165.2 | 3.4 | 13.7 | 13.8 |
| 200 | 8 | 216.3 | 4.0 | 21.2 | 21.3 |
| 250 | 10 | 267.4 | 4.0 | 26.2 | 26.4 |
| 300 | 12 | 318.5 | 4.5 | 35.2 | 35.4 |
|
|
|
Nominal Diameter 公称口径 |
Outside Diameter 外径 |
Nominal Wall Thickness 公称壁厚 |
|||
|
Wall Thickness 壁厚 |
Weight (kg/m) 重量 |
||||
|
A |
B |
Grade 钢号 |
|||
|
304 304H 304L 321 321H
|
309 309S 310 310S 316 316H 316L 316Ti 317 317L 347 347H |
||||
|
mm |
in |
mm |
mm |
||
|
6 |
1/8 |
10.5 |
1.5 |
0.336 |
0.338 |
| 8 | 1/4 | 13.8 | 2.0 | 0.588 | 0.592 |
| 10 | 3/8 | 17.3 | 2.0 | 0.762 | 0.767 |
| 15 | 1/2 | 21.7 | 2.5 | 1.20 | 1.20 |
| 20 | 3/4 | 27.2 | 2.5 | 1.54 | 1.55 |
| 25 | 1 | 34.0 | 3.0 | 2.32 | 2.33 |
| 32 | 1 1/4 | 42.7 | 3.0 | 2.97 | 2.99 |
| 40 | 1 1/2 | 48.6 | 3.0 | 3.41 | 3.43 |
| 50 | 2 | 60.5 | 3.5 | 4.97 | 5.00 |
| 65 | 2 1/2 | 76.3 | 3.5 | 6.35 | 6.39 |
| 80 | 3 | 89.1 | 4.0 | 8.48 | 8.53 |
| 90 | 3 1/2 | 101.6 | 4.0 | 9.72 | 9.79 |
| 100 | 4 | 114.3 | 4.0 | 11.0 | 11.1 |
| 125 | 5 | 139.8 | 5.0 | 16.8 | 16.9 |
| 150 | 6 | 165.2 | 5.0 | 20.0 | 20.1 |
| 200 | 8 | 216.3 | 6.5 | 34.0 | 34.2 |
| 250 | 10 | 267.4 | 6.5 | 42.2 | 42.5 |
| 300 | 12 | 318.5 | 6.5 | 50.5 | 50.8 |
|
|
|
Nominal Diameter 公称口径 |
Outside Diameter 外径 |
Nominal Wall Thickness 公称壁厚 |
|||
|
Wall Thickness 壁厚 |
Weight (kg/m) 重量 |
||||
|
A |
B |
Grade 钢号 |
|||
|
304 304H 304L 321 321H
|
309 309S 310 310S 316 316H 316L 316Ti 317 317L 347 347H |
||||
|
mm |
in |
mm |
mm |
||
|
6 |
1/8 |
10.5 |
1.7 |
0.373 |
0.375 |
| 8 | 1/4 | 13.8 | 2.2 | 0.636 | 0.640 |
| 10 | 3/8 | 17.3 | 2.3 | 0.859 | 0.865 |
| 15 | 1/2 | 21.7 | 2.8 | 1.32 | 1.33 |
| 20 | 3/4 | 27.2 | 2.9 | 1.76 | 1.77 |
| 25 | 1 | 34.0 | 3.4 | 2.59 | 2.61 |
| 32 | 1 1/4 | 42.7 | 3.6 | 3.51 | 3.53 |
| 40 | 1 1/2 | 48.6 | 3.7 | 4.14 | 4.16 |
| 50 | 2 | 60.5 | 3.9 | 5.50 | 5.53 |
| 65 | 2 1/2 | 76.3 | 5.2 | 9.21 | 9.27 |
| 80 | 3 | 89.1 | 5.5 | 11.5 | 11.5 |
| 90 | 3 1/2 | 101.6 | 5.7 | 13.6 | 13.7 |
| 100 | 4 | 114.3 | 6.0 | 16.2 | 16.3 |
| 125 | 5 | 139.8 | 6.6 | 21.9 | 22.0 |
| 150 | 6 | 165.2 | 7.1 | 28.0 | 28.1 |
| 200 | 8 | 216.3 | 8.2 | 42.5 | 42.8 |
| 250 | 10 | 267.4 | 9.3 | 59.8 | 60.2 |
| 300 | 12 | 318.5 | 10.3 | 79.1 | 79.6 |
| 350 | 14 | 355.6 | 11.1 | 95.3 | 95.9 |
| 400 | 16 | 406.4 | 12.7 | 125 | 125 |
| 450 | 18 | 457.2 | 14.3 | 158 | 159 |
| 500 | 20 | 508.0 | 15.1 | 185 | 187 |
| 550 | 22 | 558.8 | 15.9 | 215 | 216 |
| 600 | 24 | 609.6 | 17.5 | 258 | 260 |
| 650 | 26 | 660.4 | 18.9 | 302 | 304 |
|
|
|
Nominal Diameter 公称口径 |
Outside Diameter 外径 |
Nominal Wall Thickness 公称壁厚 |
|||
|
Wall Thickness 壁厚 |
Weight (kg/m) 重量 |
||||
|
A |
B |
Grade 钢号 |
|||
|
304 304H 304L 321 321H
|
309 309S 310 310S 316 316H 316L 316Ti 317 317L 347 347H |
||||
|
mm |
in |
mm |
mm |
||
|
6 |
1/8 |
10.5 |
2.4 |
0.484 |
0.487 |
| 8 | 1/4 | 13.8 | 3.0 | 0.807 | 0.812 |
| 10 | 3/8 | 17.3 | 3.2 | 1.12 | 1.13 |
| 15 | 1/2 | 21.7 | 3.7 | 1.66 | 1.67 |
| 20 | 3/4 | 27.2 | 3.9 | 2.26 | 2.28 |
| 25 | 1 | 34.0 | 4.5 | 3.31 | 3.33 |
| 32 | 1 1/4 | 42.7 | 4.9 | 4.61 | 4.64 |
| 40 | 1 1/2 | 48.6 | 5.1 | 5.53 | 5.56 |
| 50 | 2 | 60.5 | 5.5 | 7.54 | 7.58 |
| 65 | 2 1/2 | 76.3 | 7.0 | 12.1 | 12.2 |
| 80 | 3 | 89.1 | 7.6 | 15.4 | 15.5 |
| 90 | 3 1/2 | 101.6 | 8.1 | 18.9 | 19.0 |
| 100 | 4 | 114.3 | 8.6 | 22.6 | 22.8 |
| 125 | 5 | 139.8 | 9.5 | 30.8 | 31.0 |
| 150 | 6 | 165.2 | 11.0 | 42.3 | 42.5 |
| 200 | 8 | 216.3 | 12.7 | 64.4 | 64.8 |
| 250 | 10 | 267.4 | 15.1 | 94.9 | 95.5 |
| 300 | 12 | 318.5 | 17.4 | 131 | 131 |
| 350 | 14 | 355.6 | 19.0 | 159 | 160 |
| 400 | 16 | 406.4 | 21.4 | 205 | 207 |
| 450 | 18 | 457.2 | 23.8 | 257 | 259 |
| 500 | 20 | 508.0 | 26.2 | 314 | 316 |
| 550 | 22 | 558.8 | 28.6 | 378 | 380 |
| 600 | 24 | 609.6 | 31.0 | 447 | 450 |
| 650 | 26 | 660.4 | 34.0 | 531 | 534 |
|
|
|
Nominal Diameter 公称口径 |
Outside Diameter 外径 |
Nominal Wall Thickness 公称壁厚 |
|||
|
Wall Thickness 壁厚 |
Weight (kg/m) 重量 |
||||
|
A |
B |
Grade 钢号 |
|||
|
304 304H 304L 321 321H
|
309 309S 310 310S 316 316H 316L 316Ti 317 317L 347 347H |
||||
|
mm |
in |
mm |
mm |
||
|
100 |
4 |
114.3 |
11.1 |
28.5 |
28.7 |
| 125 | 5 | 139.8 | 12.7 | 40.2 | 40.5 |
| 150 | 6 | 165.2 | 14.3 | 53.8 | 54.1 |
| 200 | 8 | 216.3 | 18.2 | 89.8 | 90.4 |
| 250 | 10 | 267.4 | 21.4 | 131 | 132 |
| 300 | 12 | 318.5 | 25.4 | 185 | 187 |
| 350 | 14 | 355.6 | 27.8 | 227 | 228 |
| 400 | 16 | 406.4 | 30.9 | 289 | 291 |
| 450 | 18 | 457.2 | 34.9 | 367 | 369 |
| 500 | 20 | 508.0 | 38.1 | 446 | 449 |
| 550 | 22 | 558.8 | 41.3 | 532 | 536 |
| 600 | 24 | 609.6 | 46.0 | 646 | 650 |
| 650 | 26 | 660.4 | 49.1 | 748 | 752 |
|
|
|
Nominal Diameter 公称口径 |
Outside Diameter 外径 |
Nominal Wall Thickness 公称壁厚 |
|||
|
Wall Thickness 壁厚 |
Weight (kg/m) 重量 |
||||
|
A |
B |
Grade 钢号 |
|||
|
304 304H 304L 321 321H
|
309 309S 310 310S 316 316H 316L 316Ti 317 317L 347 347H |
||||
|
mm |
in |
mm |
mm |
||
|
15 |
1/2 |
21.7 |
4.7 |
1.99 |
2.00 |
| 20 | 3/4 | 27.2 | 5.5 | 2.97 | 2.99 |
| 25 | 1 | 34.0 | 6.4 | 4.40 | 4.43 |
| 32 | 1 1/4 | 42.7 | 6.4 | 5.79 | 5.82 |
| 40 | 1 1/2 | 48.6 | 7.1 | 7.34 | 7.39 |
| 50 | 2 | 60.5 | 8.7 | 11.2 | 11.3 |
| 65 | 2 1/2 | 76.3 | 9.5 | 15.8 | 15.9 |
| 80 | 3 | 89.1 | 11.1 | 21.6 | 21.7 |
| 90 | 3 1/2 | 101.6 | 12.7 | 28.1 | 28.3 |
| 100 | 4 | 114.3 | 13.5 | 33.9 | 34.1 |
| 125 | 5 | 139.8 | 15.9 | 49.1 | 49.4 |
| 150 | 6 | 165.2 | 18.2 | 66.6 | 67.1 |
| 200 | 8 | 216.3 | 23.0 | 111 | 111 |
| 250 | 10 | 267.4 | 28.6 | 170 | 171 |
| 300 | 12 | 318.5 | 33.3 | 237 | 238 |
| 350 | 14 | 355.6 | 35.7 | 284 | 286 |
| 400 | 16 | 406.4 | 40.5 | 369 | 372 |
| 450 | 18 | 457.2 | 45.2 | 464 | 467 |
| 500 | 20 | 508.0 | 50.0 | 570 | 574 |
| 550 | 22 | 558.8 | 54.0 | 679 | 683 |
| 600 | 24 | 609.6 | 59.5 | 815 | 821 |
| 650 | 26 | 660.4 | 64.2 | 953 | 960 |
|
Remarks: 1) The designation of the pipe shall be based on the nominal diameter and nominal wall thickness (schedule number: Sch). However, for the nominal diameter, either A (mm) or B (in) shall be used, and letter A and B shall be suffixed to the figures of nominal diameter respectively for identification. 2) The value of mass shall be calculated by the following formula and rounded off to 3 significant digits in accordance with JIS Z 8401. However, in the case of exceeding 1000 kg/m, the results shall be rounded off to an integral value of kg/m. 3) When dimensions other than those given in the abovementioned table are required, the dimensions shall be determined as agreed upon between the purchaser and supplier. |
|
Symbol of Grade 型号 |
Density 比重 kg/m2/mm |
Formulas 方程式 W : unit mass of pipe (kg/m) t : wall thickness of pipe (mm) D : outside diameter of pipe (mm) |
|
SUS304TP, SUS304HTP, SUS304LTP, SUS321TP, SUS321HTP |
7.93 |
W = 0.02491 t (D-t) |
|
SUS309TP, SUS309STP, SUS310TP, SUS310STP, SUS316TP, SUS316HTP, SUS316LTP, SUS316TiTP, SUS317TP, SUS317LTP, SUS347TP, SUS347HTP |
7.98 |
W = 0.02507 t (D-t) |