| 日本标准钢管 | |
|
|
|
| 黑钢管 |
|
| 镀锌钢管 | |
|
Nominal Bore * 公称口径 |
Outside Diameter 外径 D |
Wall Thickness ** 壁厚 t |
|||
| A | B | ||||
| mm | in | mm | in | mm | in |
| 6 | 1/8 | 10.5 | 0.413 | 2.0 | 0.079 |
| 8 | 1/4 | 13.8 | 0.543 | 2.3 | 0.091 |
| 10 | 3/8 | 17.3 | 0.681 | 2.3 | 0.091 |
| 15 | 1/2 | 21.7 | 0.854 | 2.8 | 0.110 |
| 20 | 3/4 | 27.2 | 1.071 | 2.8 | 0.110 |
| 25 | 1 | 34.0 | 1.339 | 3.2 | 0.126 |
| 32 | 1 1/4 | 42.7 | 1.681 | 3.5 | 0.138 |
| 40 | 1 1/2 | 48.6 | 1.913 | 3.5 | 0.138 |
| 50 | 2 | 60.5 | 2.382 | 3.8 | 0.150 |
| 65 | 2 1/2 | 76.3 | 3.004 | 4.2 | 0.165 |
| 80 | 3 | 89.1 | 3.508 | 4.2 | 0.165 |
| 90 | 3 1/2 | 101.6 | 4.000 | 4.2 | 0.165 |
| 100 | 4 | 114.3 | 4.500 | 4.5 | 0.177 |
| 125 | 5 | 139.8 | 5.504 | 4.5 | 0.177 |
| 150 | 6 | 165.2 | 6.504 | 5.0 | 0.197 |
| 175 | 7 | 190.7 | 7.508 | 5.3 | 0.209 |
| 200 | 8 | 216.3 | 8.516 | 5.8 | 0.228 |
| 225 | 9 | 241.8 | 9.520 | 6.2 | 0.244 |
| 250 | 10 | 267.4 | 10.528 | 6.6 | 0.260 |
| 300 | 12 | 318.5 | 12.539 | 6.9 | 0.272 |
| 350 | 14 | 355.6 | 14.000 | 7.9 | 0.311 |
| 400 | 16 | 406.4 | 16.000 | 7.9 | 0.311 |
| 450 | 18 | 457.2 | 18.000 | 7.9 | 0.311 |
| 500 | 20 | 508.0 | 20.000 | 7.9 | 0.311 |
|
Notes : 1. * For the nominal size, either A or B shall be used and letter symbol A or B shall be suffixed to the figures of nominal size to identify A or B series, respectively.
2. ** Wall thickness t tolerances plus (+) not specified and minus (-) 12.5% max.
3. The value for weight shall be calculated from the following formula assuming 7.85 g/cm3 and rounded off to 3 significant figures in accordance with JIS Z 8401 : W = 0.02466 x t x (D - t ) where W : unit mass of pipe (kg/m) t : wall thickness of pipe (mm) D : outside diameter of pipe (mm) |