Nominal Size 型号 D x B |
Thickness 厚度 t |
Unit Weight 单位重量 |
|
mm |
mm |
kg/m |
|
90 x 90
|
l3.6 4.0 5.0 6.3 8.0 |
9.66 10.7 13.1 16.2 20.1 |
|
100 x 100 |
4.0 5.0 6.3 8.0 10.0 |
11.9 14.7 18.2 22.6 27.4 |
|
120 x 120 |
5.0 6.3 8.0 10.0 12.5 |
17.8 22.2 27.6 33.7 40.9 |
|
140 x 140 |
5.0 6.3 8.0 10.0 12.5 |
21.0 26.1 32.6 40.0 48.7 |
|
150 x 150 |
5.0 6.3 8.0 10.0 12.5 ++ 16.0 |
22.6 28.1 35.1 43.1 52.7 65.2 |
|
160 x 160 |
5.0 6.3 8.0 10.0 l12.5 |
24.1 30.1 37.6 46.3 56.6 |
|
180 x 180 |
6.3 8.0 10.0 12.5 16.0 |
34.0 42.7 52.5 64.4 80.2 |
|
200 x 200 |
5.0 6.3 8.0 10.0 12.5 16.0 |
30.4 38.0 47.7 58.8 72.3 90.3 |
|
250 x 250 |
6.3 8.0 10.0 12.5 16.0 |
47.9 60.3 74.5 91.9 115 |
|
300 x 300 |
l6.3 8.0 10.0 12.5 16.0 |
57.8 72.8 90.2 112 141 |
|
350 x 350 |
8.0 10.0 12.5 16.0 + 19.0 + 22.0 + 25.0 r |
85.4 106 131 166 190 217 242 |
|
400 x 400 |
10.0 12.5 16.0 + 20.0 r + 22.0 + 25.0 |
122 151 191 235 251 282 |
|
450 x 450 |
+ 12.0 + 16.0 + 19.0 + 22.0 + 25.0 r + 28.0 r + 32.0 r |
162 213 250 286 321 355 399 |
|
500 x 500 |
+ 12.0 + 16.0 + 19.0 + 22.0 + 25.0 + 28.0 r + 32.0 r + 36.0 r |
181 238 280 320 360 399 450 498 |
|
550 x 550 |
+ 16.0 + 19.0 + 22.0 + 25.0 r + 28.0 r + 32.0 r + 36.0 r + 40.0 r |
263 309 355 399 443 500 555 608 |
|
600 x 600* |
+ 25.0 r + 28.0 r + 32.0 r + 36.0 r + 40.0 r |
439 487 550 611 671 |
|
700 x 700* |
+ 25.0 r + 28.0 r + 32.0 r + 36.0 r + 40.0 r |
517 575 651 724 797 |
|
800 x 800* |
+ 25.0 r + 28.0 r + 32.0 r + 36.0 r + 40.0 r + 45.0 r + 50.0 r + 60.0 r |
596 663 751 837 922 1026 1127 1321 |
|
l - Not in regular rolling schedule r - SAW process ++ - Hot formed from Seamless hollow + - Available in JIS G 3136 only * - 16, 19 and 22mm thickness are available on request to mill |