Nominal Size 型号 D x B |
Thickness 厚度 t |
Unit Weight 单位重量 |
|
mm |
mm |
kg/m |
|
100 x 50 |
l3.0 3.2 4.0 5.0 6.3 8.0 |
6.71 7.13 8.78 10.8 13.3 16.3 |
|
100 x 60 |
l3.6 5.0 6.3 8.0 |
8.53 11.6 14.2 17.5 |
|
120 x 60 |
3.6 5.0 6.3 8.0 |
9.66 13.1 16.2 20.1 |
|
120 x 80 |
5.0 6.3 8.0 10.0 |
14.7 18.2 22.6 27.4 |
|
150 x 100 |
5.0 6.3 8.0 10.0 l12.5 |
18.6 23.1 28.9 35.3 42.8 |
|
160 x 80 |
4.0 5.0 6.3 8.0 10.0 |
14.4 17.8 22.2 27.6 33.7 |
|
200 x 100 |
5.0 6.3 8.0 10.0 12.5 |
22.6 28.1 35.1 43.1 52.7 |
|
200 x 150 |
8.0 10.0 |
41.4 51.0 |
|
250 x 100 |
l10.0 l12.5 |
51.0 62.5 |
|
250 x 150 |
5.0 6.3 8.0 10.0 12.5 16.0 |
30.4 38.0 47.7 58.8 72.3 90.3 |
|
300 x 100 |
8.0 10.0 |
47.7 58.8 |
|
300 x 200 |
6.3 8.0 10.0 12.5 16.0 |
47.9 60.3 74.5 91.9 115 |
|
400 x 200 |
8.0 10.0 12.5 16.0 |
72.8 90.2 112 141 |
|
450 x 250
|
8.0 10.0 12.5 16.0 |
85.4 106 131 166 |
|
500 x 300 |
l8.0 10.0 l12.5 16.0 20.0 r |
97.9 122 151 191 235 |
|
l - Not in regular rolling schedule r - SAW process |