Outer Diameter 外径 D |
Thickness 厚度 t |
Unit Weight 单位重量 |
|
mm |
mm |
kg/m |
|
76.1 |
2.9 3.2 l 4.0 5.0 |
5.24 5.75 7.11 8.77 |
|
88.9 |
3.2 4.0 5.0 l 6.3 |
6.76 8.38 10.3 12.8 |
|
114.3 |
3.2 3.6 4.0 5.0 6.3 |
8.77 9.83 10.9 13.5 16.8 |
|
139.7 |
5.0 6.3 8.0 10.0 |
16.6 20.7 26.0 32.0 |
|
168.3 |
5.0 6.3 8.0 10.0 |
20.1 25.2 31.6 39.0 |
|
193.7 |
5.0 6.3 8.0 10.0 |
23.3 29.1 36.6 45.3 |
|
219.1 |
l 5.0 6.3 l 8.0 10.0 l 12.5 |
26.4 33.1 41.6 51.6 63.7 |
|
244.5 |
l 8.0 l 10.0 l 12.5 16.0 |
46.7 57.8 71.5 90.2 |
|
273.0 |
6.3 l 8.0 l 10.0 l 12.5 l 16.0 |
41.4 52.3 64.9 80.3 101 |
|
323.9 |
6.3 l 8.0 10.0 12.5 16.0 |
49.3 62.3 77.4 96.0 121 |
|
355.6 |
l 16.0 |
134 |
|
406.4 |
l 12.5 l 16.0 |
121 154 |
|
457 |
l 16.0 |
174 |
|
508 |
l 10.0 l 16.0 |
123 194 |
|
l - Not in regular rolling schedule |