Outer Diameter 外径 D |
Thickness 厚度 t |
Unit Weight 单位重量 |
| mm |
mm |
kg/m |
| 76.1 |
2.5 3.0 4.0 |
4.54 5.41 7.11 |
| 88.9 |
3.0 3.5 4.0 5.0 |
6.36 7.37 8.38 10.3 |
| 114.3 |
3.0 3.5 4.0 5.0 6.0 |
8.23 9.56 10.9 13.5 16.0 |
| 139.7 |
4.0 5.0 6.0 8.0 10.0 |
13.4 16.6 19.8 26.0 32.0 |
| 168.3 |
4.0 5.0 6.0 8.0 10.0 12.5 |
16.2 20.1 24.0 31.6 39.0 48.0 |
| 193.7 |
4.0 4.5 5.0 6.0 8.0 10.0 12.5 |
18.7 21.0 23.3 27.8 36.6 45.3 55.9 |
| 219.1 |
4.5 5.0 6.0 8.0 10.0 12.0 12.5 16.0 |
23.8 26.4 31.5 41.6 51.6 61.3 63.7 80.1 |
|
244.5 |
5.0 6.0 8.0 10.0 12.0 12.5 16.0 |
29.5 35.3 46.7 57.8 68.8 71.5 90.2 |
|
273.0 |
5.0 6.0 8.0 10.0 12.0 12.5 16.0 |
33.0 39.5 52.3 64.9 77.2 80.3 101 |
|
323.9 |
5.0 6.0 8.0 10.0 12.0 12.5 16.0 |
39.3 47.0 62.3 77.4 92.3 96.0 121 |
|
355.6 |
5.0 6.0 8.0 10.0 12.0 12.5 16.0 |
43.2 51.7 68.6 85.2 102 106 134 |
|
406.4 |
6.0 8.0 10.0 12.0 12.5 16.0 |
59.2 78.6 97.8 117 121 154 |
|
457 |
6.0 8.0 10.0 12.0 12.5 16.0 |
66.7 88.6 110 132 137 174 |
|
508 |
6.0 8.0 10.0 12.0 12.5 16.0 |
74.3 98.6 123 147 153 194 |