| C型轻量槽钢 |
|
Serial Size 型号 D x B |
Thickness 厚度 t |
Unit Weight 单位重量 |
| mm | mm | kg/m |
|
60 x 30 |
1.6 2.3 |
1.44 2.03 |
|
75 x 45 |
1.6 2.3 3.0 |
2.00 2.84 3.65 |
|
100 x 50 |
1.6 2.3 3.0 |
2.44 3.47 4.47 |
|
125 x 50 |
2.3 3.0 4.5 |
3.92 5.06 7.42 |
|
150 x 65 |
2.3 3.0 4.0 4.5 |
4.91 6.36 8.38 9.36 |
|
175 x 75 |
2.3 3.0 4.0 4.5 |
5.73 7.42 9.79 10.95 |
|
200 x 75 |
2.3 3.0 4.0 4.5 |
6.18 8.01 10.58 11.84 |
|
225 x 75 |
2.3 3.0 4.0 4.5 |
6.63 8.59 11.36 12.72 |
|
250 x 75 |
2.3 3.0 4.0 4.5 |
7.08 9.18 12.15 13.60 |