槽鋼

Serial Size

型号

Depth x Width

D x B

Thickness

厚度

Unit Weight

单位重量

Web

t

Flange

T

mm mm kg/m lb/ft

75 x 40

3.8

6.1

5.92

3.98

100 x 50

100 x 50

100 x 50

101.6 x 76.2

4.2

5.0

5.0

7.6

6.7

8.5

8.4

9.5

8.33

10.2

10.1

16.6

5.60

6.85

6.79

11.15

120 x 55

125 x 65

125 x 65

5.5

4.7

5.5

9.1

7.5

9.5

12.5

11.9

14.8

8.40

8.00

9.94

140 x 60

150 x 75

150 x 75

150 x 90

160 x 65

6.0

6.0

5.5

6.5

6.5

9.9

9.5

10.0

12.0

10.4

15.3

17.7

17.9

23.9

18.1

10.28

11.89

12.03

16.06

12.16

180 x 70

180 x 75

180 x 75

180 x 90

7.0

6.0

6.0

6.5

10.9

11.0

10.5

12.5

21.1

20.9

20.3

26.1

14.18

14.04

13.64

17.54

200 x 75

200 x 75

200 x 75

200 x 90

7.5

6.0

6.0

7.0

11.4

12.0

12.5

14.0

24.3

22.9

23.4

29.7

16.33

15.39

15.72

19.96

220 x 80

230 x 75

230 x 75

230 x 90

7.9

6.5

6.5

7.5

12.5

12.0

12.5

14.0

28.3

25.1

25.7

32.2

19.02

16.87

17.27

21.64

240 x 85

250 x 90

260 x 75

260 x 90

260 x 90

280 x 95

8.4

8.0

7.0

8.0

8.8

9.2

13.0

15.0

12.0

14.0

13.9

14.8

32.0

35.5

27.6

34.8

36.3

40.9

21.50

23.85

18.55

23.38

24.39

27.48

300 x 90

300 x 90

300 x 100

300 x 100

8.0

9.0

9.0

9.6

16.0

15.5

16.5

15.5

40.1

41.4

45.5

45.4

26.94

27.82

30.57

30.51

380 x 100

380 x 100

10.0

9.5

17.5

17.5

55.2

54.0

37.09

36.28

430 x 100

11.0

19.0

64.4

43.27