Serial Size 型号 D x B x C |
Thickness 厚度 t |
Unit Weight 单位重量 |
| mm | mm | kg/m |
|
60 x 30 x 10 |
1.6 2.0 2.3 |
1.63 1.99 2.25 |
|
75 x 45 x 15 |
1.6 2.0 2.3 3.0 |
2.32 2.86 3.25 4.13 |
|
100 x 50 x 20 |
1.6 2.0 2.3 2.6 2.8 3.0 3.2 4.0 4.5 |
2.88 3.56 4.06 4.55 4.87 5.18 5.50 6.71 7.43 |
|
125 x 50 x 20 |
2.0 2.3 3.0 3.2 4.0 4.5 |
3.95 4.51 5.77 6.13 7.50 8.32 |
|
150 x 50 x 20 |
2.3 3.2 4.5 |
4.96 6.76 9.20 |
|
150 x 65 x 20 |
2.3 3.0 3.2 4.0 4.5 |
5.50 7.07 7.51 9.22 10.25 |
|
175 x 75 x 20 |
2.3 3.0 3.2 4.0 4.5 |
6.31 8.13 8.63 10.63 11.84 |
|
200 x 75 x 20 |
2.3 3.0 3.2 4.0 4.5 |
6.76 8.71 9.27 11.4 12.7 |
|
200 x 75 x 25 |
2.3 3.0 3.2 4.0 4.5 |
6.95 8.96 9.52 11.7 13.1 |
|
225 x 75 x 20 |
2.3 3.0 3.2 4.0 4.5 |
7.21 9.30 9.90 12.19 13.60 |
|
225 x 75 x 25 |
2.3 3.0 3.2 4.0 4.5 |
7.40 9.54 10.15 12.50 14.00 |
|
250 x 75 x 20 |
3.0 3.2 4.0 4.5 |
9.89 10.52 12.96 14.50 |
|
250 x 75 x 25 |
3.0 3.2 4.0 4.5 |
10.13 10.96 13.00 14.90 |