工字钢(欧洲标准)
|
|
Serial Size 型号 |
Depth X Width D X B |
Unit Weight 单位重量 |
Thickness 厚度 |
Radius 半径 |
||
| Web t | Flange T | Root r1 | Toe r2 | |||
| mm | kg/m | mm | mm | mm | mm | |
|
IPN 80 |
80 X 42 |
5.94 |
3.9 |
5.9 |
3.9 |
2.3 |
|
IPN 100 |
100 x 50 |
8.34 |
4.5 |
6.8 |
4.5 |
2.7 |
|
IPN 120 |
120 x 58 |
11.1 |
5.1 |
7.7 |
5.1 |
3.1 |
|
IPN 140 |
140 x 66 |
14.3 |
5.7 |
8.6 |
5.7 |
3.4 |
|
IPN 160 |
160 x 74 |
17.9 |
6.3 |
9.5 |
6.3 |
3.8 |
|
IPN 180 |
180 x 82 |
21.9 |
6.9 |
10.4 |
6.9 |
4.1 |
|
IPN 200 |
200 x 90 |
26.2 |
7.5 |
11.3 |
7.5 |
4.5 |
|
IPN 220 |
220 x 98 |
31.1 |
8.1 |
12.2 |
8.1 |
4.9 |
|
IPN 240 |
240 x 106 |
36.2 |
8.7 |
13.1 |
8.7 |
5.2 |
|
IPN 260 |
260 x 113 |
41.9 |
9.4 |
14.1 |
9.4 |
5.6 |
|
IPN 280 |
280 x 119 |
47.9 |
10.1 |
15.2 |
10.1 |
6.1 |
|
IPN 300 |
300 x 125 |
54.2 |
10.8 |
16.2 |
10.8 |
6.5 |
|
IPN 320 |
320 x 131 |
61.0 |
11.5 |
17.3 |
11.5 |
6.9 |
|
IPN 340 |
340 x 137 |
68.0 |
12.2 |
18.3 |
12.2 |
7.3 |
|
IPN 360 |
360 x 143 |
76.1 |
13 |
19.5 |
13 |
7.8 |
|
IPN 380 |
380 x 149 |
84.0 |
13.7 |
20.5 |
13.7 |
8.2 |
|
IPN 400 |
400 x 155 |
92.4 |
14.4 |
21.6 |
14.4 |
8.6 |
|
IPN 450 |
450 x 170 |
115 |
16.2 |
24.3 |
16.2 |
9.7 |
|
IPN 500 |
500 x 185 |
141 |
18 |
27 |
18 |
10.8 |
|
IPN 550 |
550 x 200 |
166 |
19 |
30 |
19 |
11.9 |