工字椿

Serial Size

型号

D x B

Unit Weight

单位重量

Depth of Section

D

Width of Section

B

Thickness

厚度

Web t = Flange T

mm / in kg/m lb/ft mm in mm in mm in

356 x 406   UP

( 14 x 16 )         

175.6

118.0

360.0

14.173

396.0

15.591

20.0

0.787

400 x 400  1971

(JIS SERIES ONLY)  1971

1971

197

168

140

132.37

112.89

94.07

400.0

394.0

388.0

15.748

15.512

15.276

408.0

405.0

402.0

16.063

15.945

15.827

21.0

18.0

15.0

0.827

0.709

0.591

356 x 368       UP

(14 X 14 1/2) HP14

HP14

HP14

HP14

180.07

174.12

151.80

132.45

108.64

121

117

102

89

73

362.9

360.9

355.9

351.3

345.7

14.287

14.209

14.012

13.831

13.610

378.8

378.1

375.5

373.3

370.5

14.913

14.886

14.783

14.697

14.587

21.1

20.4

17.9

15.6

12.8

0.831

0.803

0.705

0.614

0.504

350 x 350    1971

(JIS SERIES ONLY) 1994

1971

1994

1971

1994

156

154

131

129

106

105

104.82

103.48

88.02

86.88

71.23

70.55

350

350

344

344

338

338

13.780

13.780

13.543

13.543

13.307

13.307

357

357

354

354

351

351

14.055

14.055

13.937

13.937

13.819

13.819

19

19

16

16

13

13

0.748

0.748

0.630

0.630

0.512

0.512

330 x 330    HP13

(13 x 13)     HP13

(Not in regular    HP13

rolling schedule)   HP13

148.82

129.47

108.64

89.29

100

87

73

60

334.0

328.9

323.8

318.5

13.150

12.949

12.748

12.539

335.4

332.9

330.3

327.7

13.205

13.106

13.004

12.902

19.4

16.9

14.4

11.7

0.765

0.665

0.565

0.460

305 x 305   HP12

(12 x 12)    HP12

UP

UP

HP12

UP

UP

HP12

HP12

UP

HP12

UP

HP12

282.76

252.99

221.74

186.02

180.07

148.82

126.50

125.01

110.13

95.24

93.76

87.80

78.87

190

170

149

125

121

100

85

84

74

64

63

59

53

365.3

356.4

337.9

328.3

326.7

318.5

312.6

311.9

308.1

303.8

303.3

301.7

299.2

14.380

14.030

13.303

12.925

12.862

12.539

12.307

12.280

12.130

11.961

11.941

11.878

11.780

321.8

319.3

325.7

320.9

319.7

316.0

312.7

312.3

310.3

308.3

308.0

307.8

305.9

12.670

12.570

12.823

12.634

12.587

12.441

12.311

12.295

12.217

12.138

12.126

12.118

12.043

44.1

39.6

30.3

25.5

24.8

20.6

17.8

17.4

15.4

13.4

13.1

12.4

11.0

1.735

1.560

1.193

1.004

0.976

0.811

0.701

0.685

0.606

0.528

0.516

0.488

0.433

300 x 300   1971

(JIS SERIES ONLY) 1994

1971

1994

106

105

84.5

83.4

71.23

70.55

56.78

56.04

300

300

294

294

11.811

11.811

11.575

11.575

305

305

302

302

12.008

12.008

11.890

11.890

15

15

12

12

0.591

0.591

0.472

0.472

254 x 254   HP10

(10 x 10)        UP

HP10

84.83

71.43

62.50

57

48

42

253.7

249.7

246.4

9.988

9.831

9.701

259.7

258.0

255.9

10.224

10.157

10.075

14.4

12.0

10.5

0.567

0.472

0.413

250 x 250   1971

(JIS SERIES ONLY) 1994

1971

1994

82.2

81.6

64.5

63.8

55.23

54.83

43.34

42.87

250

250

244

244

9.843

9.843

9.606

9.606

255

255

252

252

10.039

10.039

9.921

9.921

14

14

11

11

0.551

0.551

0.433

0.433

203 x 203   HP8

(8 x 8)        UP

53.57

44.65

36

30

203.7

200.2

8.020

7.882

207.1

205.9

8.154

8.106

11.3

9.5

0.445

0.374

200 x 200  1971

       (JIS SERIES ONLY) 

56.2

37.76

200

7.874

204

8.031

12

0.472