方钢

Side Length

长度

Unit Weight

单位重量

mm  in kg/m

6

0.236

0.28

8

0.315

0.50

9

0.354

0.64

10

0.394

0.79

12

0.472

1.13

13

0.512

1.33

15

0.591

1.77

16

0.630

2.01

18

0.709

2.54

19

0.748

2.83

20

0.787

3.14

22

0.866

3.80

24

0.945

4.52

25

0.984

4.91

28

1.102

6.15

30

1.181

7.07

32

1.260

8.04

36

1.417

10.2

38

1.496

11.3

40

1.575

12.6

42 1.654 13.8
44 1.732 15.2
46 1.811 16.6
50 1.969 19.6
55 2.165 23.7
60 2.362

28.3

65 2.559 33.2
75 2.953 44.2
90 3.543 63.6
100 3.937 78.5
120 4.724 113.0
130 5.118 133.0
140 5.512 154.0
160 6.299 177.0