Nominal
Diameter
公称口径 |
Unit
Weight
单位重量 |
Mass(质量)
per 12m Run |
| mm |
kg/m |
kg |
|
6 |
0.222 |
2.664 |
| l
8 |
0.395 |
4.740 |
|
9 |
0.499 |
5.988 |
| 10 |
0.616 |
7.392 |
|
12 |
0.888 |
10.656 |
|
13 |
1.042 |
12.504 |
|
14 |
1.208 |
14.496 |
|
16 |
1.579 |
18.948 |
|
18 |
1.998 |
23.976 |
| l
19 |
2.230 |
26.760 |
|
20 |
2.466 |
29.592 |
|
22 |
2.984 |
35.808 |
| l
24 |
3.550 |
42.600 |
| 25 |
3.854 |
46.248 |
| 28 |
4.834 |
58.008 |
| 32 |
6.313 |
75.756 |
|
35 |
7.553 |
90.636 |
| 38 |
8.903 |
106.836 |
| l
40 |
9.864 |
118.368 |
| l
50 |
15.413 |
184.956 |
l Not
in Regular Rolling Schedule.
High
Tensile Deformed Bar in 12 metres straight.
Mild
Steel Round Bar in 12 metres straight or 12 metres one fold.
Notes:
1) Carbon Equivalent CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15
2) d = Nominal Diameter
3) So = The original cross-sectional area of the test piece. |