不等边角钢

Serial Size 

型号

D x B x t

Unit Weight

单位重量

mm

kg/m lb/ft

60 x 50 x 5 

 7 

4.16

5.66

2.80

3.80

65 x 50 x 5 

4.36

5.16

5.94

7.49

2.93

3.47

3.99

5.03

70 x 60 x 6 

10 

5.91

7.66

9.42

3.97

5.15

6.33

75 x 50 x 6 

10 

5.67

7.35

9.03

3.81

4.94

6.07

75 x 65 x 6

8

10

6.38

8.29

10.2

4.29

5.57

6.85

80 x 60 x 6 

10

6.38

8.29

10.2

4.29

5.57

6.85

80 x 70 x 6 

12 

6.85

9.96

13.0

4.60

6.69

8.74

90 x 60 x 6 

12 

6.85

9.96

13.0

4.60

6.69

8.74

90 x 75 x 6 

12 

7.56

11.0

14.4

5.08

7.39

9.68

90 x 80 x 7 

10 

13 

9.04

12.6

16.0

6.07

8.47

10.75

100 x 65 x 7 

10 

11 

12 

8.77

9.94

11.1

12.3

13.4

14.4

5.89

6.68

7.46

8.26

9.00

9.68

100 x 75 x 6 

10 

11 

12 

13 

7.98

9.32

10.6

11.8

13.0

14.3

15.4

16.5

5.36

6..26

7.12

7.93

8.74

9.61

10.35

11.09

100 x 80 x 7 

10 

13 

9.59

13.3

17.0

6.44

8.94

11.4

100 x 90 x 7 

10 

13 

10.1

14.1

18.1

6.79

9.47

12.16

120 x 80 x 8 

10 

12 

12.2

15.0

17.8

8.20

10.08

11.96

125 x 75 x 7 

10 

11 

12 

13 

10.7

12.2

13.6

15.0

16.4

17.8

19.1

7.19

8.20

9.14

10.08

11.02

11.96

12.83

125 x 90 x 7 

10 

13 

11.5

16.1

20.6

7.73

10.82

13.84

130 x 65 x 8 

10 

11.8

14.6

7.93

9.81

150 x 75 x 7 

10 

11 

12 

13 

15 

12.1

15.3

17.0

18.6

20.2

21.8

24.8

8.13

10.28

11.42

12.50

13.57

14.61

16.66

150 x 90 x 8 

10 

11 

12 

15 

14.3

16.4

18.2

19.9

21.6

26.6

9.61

11.02

12.23

13.37

14.51

17.87

150 x 100 x 9 

10 

12 

14 

15 

17.1

19.0

22.4

26.1

27.7

11.49

12.77

15.05

17.54

18.61

160 x 80 x 10 

12 

18.2

21.6

12.23

14.51

175 x 90 x 9 

12 

15 

18.2

23.8

29.4

12.23

15.99

19.75

200 x 100 x 10 

12 

14 

15 

23.0

27.3

31.6

33.7

15.45

18.34

21.23

22.64

200 x 150 x 12 

15 

18 

32.0

39.6

47.1

21.50

26.61

31.65