等边角钢

Serial Size

  型号

D x B x t

Unit Weight

单位重量

mm

kg/m

lb/ft

20 x 20 x 3

0.89

0.59

25 x 25 x 3

4

5

1.12

1.45

1.77

0.75

0.97

1.19

30 x 30 x 3

4

5

1.36

1.78

2.16

0.91

1.20

1.45

40 x 40 x 3

4

5

6

1.83

2.41

2.95

3.49

1.23

1.62

1.98

2.35

45 x 45 x 3

4

5

2.11

2.74

3.38

1.42

1.84

2.27

50 x 50 x 3

4

5

6

8

2.33

3.06

3.77

4.43

5.78

1.57

2.06

2.53

2.98

3.88

60 x 60 x 4

5

6

3.68

4.55

5.41

2.47

3.06

3.64

63 x 63 x 5

6

8

4.81

5.72

7.47

3.23

3.84

5.02

65 x 65 x 5

6

8

   10

5.00

5.91

7.66

9.42

3.36

3.97

5.15

6.33

70 x 70 x 5

6

7

5.37

6.38

7.35

3.61

4.29

4.94

75 x 75 x 5

6

8

9

12

5.76

6.85

8.92

9.96

13.0

3.87

4.60

5.99

6.69

8.74

80 x 80 x 6

7

8

9

10

12

7.32

8.50

9.55

10.7

11.9

13.9

4.92

5.71

6.42

7.19

8.00

9.34

90 x 90 x 6

7

8

9

10

12

13

16

8.28

9.59

10.9

12.1

13.3

15.9

17.0

20.7

5.56

6.44

7.32

8.13

8.94

10.68

11.42

13.91

100 x 100 x 6

7

8

9

10

12

13

15

9.22

10.7

12.1

13.5

14.9

17.8

19.1

21.9

6.20

7.19

8.13

9.07

10.01

11.96

12.83

14.72

110 x 110 x 8

10

12

16

13.4

16.6.

19.7

25.8

9.00

11.15

13.24

17.34

120 x 120 x 8

10

11

12

13

15

14.7

18.2

19.9

21.5

23.3

26.6

9.88

12.23

13.37

14.45

15.66

17.87

125 x 125 x 8

10

12

16

14.9

18.0

22.5

29.1

10.01

12.09

15.12

19.55

130 x 130 x 8

9

10

11

12

15

16

16.0

17.9

19.7

21.5

23.4

28.8

30.8

10.75

12.03

13.24

14.45

15.72

19.35

20.70

150 x 150 x 10

11

12

14

15

16

18

19

22.9

25.1

27.3

31.5

33.6

35.7

40.1

41.9

15.39

16.87

18.34

21.23

22.58

23.99

26.94

28.15

160 x 160 x 14

15

16

17

18

19

34.1

36.2

38.4

40.7

42.9

45.1

22.91

24.32

25.80

27.35

28.83

30.30

175 x 175 x 12

15

31.8

39.4

21.37

26.47

180 x 180 x 13

14

15

16

17

18

19

20

35.7

38.3

40.9

43.5

46.0

48.6

51.5

53.7

23.99

25.74

27.48

29.23

30.91

32.66

34.60

36.08

200 x 200 x 13

15

16

18

20

24

25

26

40.0

45.3

48.5

54.2

59.7

71.1

73.6

76.8

26.88

30.44

32.59

36.42

40.11

47.77

49.45

51.60

250 x 250 x 25

28

32

35

93.7

104

118

128

62.96

69.88

79.29

86.01

300 x 300 x 35

155

104.15

350 x 350 x 35

182

122.29